    Hey guys. The current head on my van has a valve seat that drops every once in a while, so I am preparing to put a new head on. I have a spare swirl turbo head that is a non-oem unit with the non-magnetic exhaust valves. In photo one there is a casting error in the bowl. It doesn't touch the fire ring area, what do you guys think? Anything this may cause? Second photo is where i smoothed out the flaw. Third photo is me taking a shot at mildly de-shrouding the valves with a carbide bur (It's mild as I don't want to reduce the compression much). I made some sheet metal pieces that covered the valves and also used a scribe to be sure the deshrouding is all the same distance outwards. I still need to smooth it out with sanding rolls. Feel free to tell me if I did anything wrong. I will do the same to the other 3 chambers, and then turn my attention to the runners. For that I will take the valves/ seals out.





    Last edited by jefo; 10-11-2015 at 10:59 PM.

  2. #2
    turbo addict
    Join Date
    Jan 2006
    Location
    Hazelwood, MO
    Posts
    6,566

    Re: Swirl Head Porting for the first time and head casting defect

    That's not a "flaw" so to speak as it's more than likely something having to do with part location during machining. I have seen this on EVERY head I've ever messed with.

    I will let the more experience "magic" people speak up to the rest of what you asked, but that's what I know....

  3. #3
    The moderately moderate moderator Turbo Mopar Staff
    Join Date
    Dec 2006
    Location
    Akron, Ohio
    Posts
    6,870

    Re: Swirl Head Porting for the first time and head casting defect

    I too have seen this on every head I have ever seen on the turbo cars.
    Bryan
    86 GLHS #161, 2016 Impala
    SDAC National Member, SDAC Buckeye Chapter Member

    A man has got to know his limitations.....

  4. #4
    Supporting Member Turbo Mopar Contributor zin's Avatar
    Join Date
    May 2006
    Location
    ca
    Posts
    4,479

    Re: Swirl Head Porting for the first time and head casting defect

    I've seen it too, not to say that rounding off those sharp corners isn't a good idea...

    I would try to give it a bit more of an "undercut" to help turn the air towards the piston, rather than allowing it to "crash" into the cylinder wall though. A smallish ball rotary file should do the job, probably 1/4 to 3/8", hard to tell by the picture, and even harder to tell by memory! :-)

    Mike
    "The Constitution is not an instrument for the government to restrain the people, it is an instrument for the people to restrain the government - lest it come to dominate our lives and interests." - Patrick Henry

    Bad laws are the worst sort of tyranny.
    - Edmund Burke

  5. #5
    turbo addict
    Join Date
    Jan 2006
    Location
    Hazelwood, MO
    Posts
    6,566

    Re: Swirl Head Porting for the first time and head casting defect

    Just to give a little more feedback, I have done chamber work to 3 heads...all of them had this "feature". I blended them all into the chamber as well as knocked all of the sharp edges down to prevent hot spots. I also have eliminated the "point" in the center of the 2 valves on a swirl head, but I'm not too sure that was the best idea anymore. However, laying back the quench pad from the valves is a GOOD thing....allowing more low/mid lift flow....which is HUGE!

  6. #6
    Hybrid booster
    Join Date
    Dec 2010
    Location
    Detroit MI
    Posts
    393

    Re: Swirl Head Porting for the first time and head casting defect

    Well I only deshrouded the valves(finished with 180 grit) and port matched the runners to the gasket, trying to mimic other ported heads I have seen. I didn't touch the bowl area or very far in the runners. Let me know what you think. I'll be installing it soon.




  7. #7
    Rhymes with tortoise. Turbo Mopar Staff cordes's Avatar
    Join Date
    Dec 2005
    Location
    Tuscola, IL
    Posts
    21,469

    Re: Swirl Head Porting for the first time and head casting defect

    I'm no expert, but wouldn't not working on the bowls and runners leave most of the benefits of chamber work unrealized?

  8. #8
    boostaholic Turbo Mopar Contributor
    Join Date
    Mar 2013
    Location
    Columbia City, Indiana
    Posts
    1,222

    Re: Swirl Head Porting for the first time and head casting defect

    Quote Originally Posted by cordes View Post
    I'm no expert, but wouldn't not working on the bowls and runners leave most of the benefits of chamber work unrealized?
    I'm certainly no expert either, but I would agree with you. I've not attempted to port a swirl head(yet), but when I did the G head on my Scamp, I spent 75% of my time on the ports. The casting bosses for the head bolts are a major restrictor on several, if not most, of the ports. I spent a lot of time removing metal, and reshaping the sides & roof of the ports. It was my first time, and I really don't know if they are "right" or not. I went off of pictures and information I had found in various sources over the years.

    I can tell you this much, it runs like a raped ape, and winds to 7K without any struggle, so I must have done something right....

    That being said, I know porting for a turbo motor can be a whole different animal than N/A. Hopefully some more experienced porters will chime in...

  9. #9
    Supporting Member II Turbo Mopar Contributor ajakeski's Avatar
    Join Date
    Sep 2007
    Location
    SE Wisconsin
    Posts
    2,624

    Re: Swirl Head Porting for the first time and head casting defect

    I ported the head on my GLH including the intake and exhaust bowls under the valve. I used a ported Direct Connection head as my guide and spent a lot of time removing material.
    When you remove the valves you can see an offset between the runner and the bowl. This offset is what induces the swirl effect. If you make a radical change to this shape, you will lose the swirl effect and may cause poor flow characteristics in the port.
    I also deshrouded the valves more and smoothed the combustion chamber. Deshrouding allows for better flow when the intake valve opens. Smoothing may help reduce detonation points.

  10. #10
    Hybrid booster
    Join Date
    Dec 2010
    Location
    Detroit MI
    Posts
    393

    Re: Swirl Head Porting for the first time and head casting defect

    I was under the impression that de-shrouding the valves had a big effect of flow. But it makes sense the runners are where most of the gain is. I just needed to replace the old head and figured I do some quick (relatively) port matching and deshrouding.

  11. #11
    Supporting Member Turbo Mopar Contributor mopar-tech's Avatar
    Join Date
    Dec 2005
    Location
    Oakdale CT
    Posts
    2,419

    Re: Swirl Head Porting for the first time and head casting defect

    Quote Originally Posted by jefo View Post
    I was under the impression that de-shrouding the valves had a big effect of flow.
    On the swirl head making changes to the shape of the chamber can modify the pressure spike inherent in the design which can reduce detonation.


    Working on clearing the decks.

  12. #12
    Supporting Member Turbo Mopar Contributor
    Join Date
    Feb 2015
    Location
    toronto
    Posts
    1,767

    Re: Swirl Head Porting for the first time and head casting defect

    Quote Originally Posted by mopar-tech View Post
    On the swirl head making changes to the shape of the chamber can modify the pressure spike inherent in the design which can reduce detonation.
    Do you have a picture of before and after? To help me better understand
    Thanks!

  13. #13
    boostaholic Turbo Mopar Contributor
    Join Date
    Mar 2013
    Location
    Columbia City, Indiana
    Posts
    1,222

    Re: Swirl Head Porting for the first time and head casting defect

    Quote Originally Posted by jefo View Post
    I was under the impression that de-shrouding the valves had a big effect of flow. But it makes sense the runners are where most of the gain is. I just needed to replace the old head and figured I do some quick (relatively) port matching and deshrouding.
    It can have a big effect on flow at low lift. It can dramatically improve the "area under the curve", but without supporting mods in the bowl and ports, it may not do that much for you. Port velocity, and flow require a systematic approach. It why you don't use a set of Edelbrock heads on a small block and still run the stock 2 bbl carb... Those better heads can't do their job without the rest of the system balanced.

    It's the same reason our 2 piece intakes are so sought after. A fully ported head isn't going to show it's full potential with a 1 piece intake, it just can't flow enough(well, at least without serious modification).

    Will the de-shrouding you did help a little? Sure. At low lift you're not maxing out the port potential, but it won't do everything it can, without balancing everything in front of it.

  14. #14
    Hybrid booster
    Join Date
    Dec 2010
    Location
    Detroit MI
    Posts
    393

    Re: Swirl Head Porting for the first time and head casting defect

    I guess I will have to find out what the difference is with testing! The head and a hybrid turbo (46 trim, stage 1 .63) are on and it pulls 21 hg at idle. sweet!

  15. #15
    turbo addict
    Join Date
    Dec 2005
    Location
    WI
    Posts
    1,565

    Re: Swirl Head Porting for the first time and head casting defect

    Quote Originally Posted by mopar-tech View Post
    On the swirl head making changes to the shape of the chamber can modify the pressure spike inherent in the design which can reduce detonation.
    Pretty sure what is being said here is that deshrouding (too much) can have a negative effect, too. The 782 is a "fast burn" design. What that means is that the combustion event happens quickly is terms of crank degrees. The faster the combustion event can complete typically means the chance of detonation is reduced. As the chamber grows in size, through excessive porting, deshrouding, etc ... the spark must advance to keep peak cylinder pressure @ around 14* ATDC where the piston will induce the most power/torque. By advancing the spark, we've extended the combustion process in crank degrees which allows more time for hot spots within the chamber (plug tips, hot carbon deposits, exhaust valves) to react with the air/fuel mixture. The result being a chamber that is more prone to detonation and/or pre-ignition.

  16. #16
    turbo addict
    Join Date
    Dec 2005
    Location
    Pickering, ontario
    Posts
    2,670

    Re: Swirl Head Porting for the first time and head casting defect

    Quote Originally Posted by puppet View Post
    Pretty sure what is being said here is that deshrouding (too much) can have a negative effect, too. The 782 is a "fast burn" design. What that means is that the combustion event happens quickly is terms of crank degrees. The faster the combustion event can complete typically means the chance of detonation is reduced. As the chamber grows in size, through excessive porting, deshrouding, etc ... the spark must advance to keep peak cylinder pressure @ around 14* ATDC where the piston will induce the most power/torque. By advancing the spark, we've extended the combustion process in crank degrees which allows more time for hot spots within the chamber (plug tips, hot carbon deposits, exhaust valves) to react with the air/fuel mixture. The result being a chamber that is more prone to detonation and/or pre-ignition.

    This is exactly what I found when I went a little too much on valve deshrouding. I regret touching the chambers at all, and overall, this head has never been able to match the previous head for peak torque and horsepower numbers on the same dyno.

  17. #17
    Supporting Member II Turbo Mopar Contributor ajakeski's Avatar
    Join Date
    Sep 2007
    Location
    SE Wisconsin
    Posts
    2,624

    Re: Swirl Head Porting for the first time and head casting defect

    Here are some cut aways of the intake and exhaust ports. Helpful to have when porting.





    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_0436.JPG 
Views:	1464 
Size:	160.0 KB 
ID:	56634   Click image for larger version. 

Name:	IMG_0437.JPG 
Views:	1202 
Size:	172.1 KB 
ID:	56635   Click image for larger version. 

Name:	IMG_0438.JPG 
Views:	1023 
Size:	150.9 KB 
ID:	56636   Click image for larger version. 

Name:	IMG_0439.JPG 
Views:	951 
Size:	157.1 KB 
ID:	56637  

  18. #18
    Supporting Member II Turbo Mopar Contributor jeff1234's Avatar
    Join Date
    Mar 2006
    Location
    Albany Wisconsin
    Posts
    1,015

    Re: Swirl Head Porting for the first time and head casting defect

    Even though this thread is 5 years old I think it is important to note that in the pictures of his porting work yon need to look at the fire ring areas by the raised area for the spark plug. You will notice erosion near the fire ring. This is caused by detonation. If the head isnt milled to eliminate this, it will continue to detonate, ultimately killing the head, pistons and related parts. I know this because I am presently working on the same problem
    The only substitute for cubic inches is cubic dollars, how fast can you afford to go?

Similar Threads

  1. General SRT-4 head, swirl head, 90 big brakes, one piece valve covers, TBI parts
    By moparman76_69 in forum Parts For Sale
    Replies: 14
    Last Post: 11-24-2011, 02:05 PM
  2. Casting 655 cylinder head
    By Dez in forum Engine - Block, Piston, Heads, Intakes
    Replies: 36
    Last Post: 03-13-2008, 07:17 AM
  3. First impressions-G head VS Swirl head on my van!
    By turbovanmanČ in forum Engine - Block, Piston, Heads, Intakes
    Replies: 35
    Last Post: 08-18-2006, 01:45 PM
  4. G-head VS Swirl head valve lengths and possible way to use Swirl in G head!
    By turbovanmanČ in forum Engine - Block, Piston, Heads, Intakes
    Replies: 7
    Last Post: 08-14-2006, 04:27 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •